Name of Product
|
J I S
AWS
|
Feature
|
Use
|
|
TA-100
|
BA4045
|
Its fusion point is especially low
at the work progress temperature of aluminum-silicon
alloy.
|
Because its fusion point is low, it
is used to weld the thin board of aluminum and aluminum
alloys. It can be also used for a narrow gap part.
|
|
TA-101
|
BA1-1
|
Its low silicon content is favorable
to strengthen the welded part.
|
It is proper to weld aluminum and
the boards and pipe of aluminum alloys
|
|
TA-102
|
BA4343
|
Its technical quality is excellent,
its fusion point is low, and its appearance is fine.
|
It is proper to weld aluminum and
the boards and pipe of aluminum alloys
|
|
TA-103
|
BA4145
|
This is an aging treatment alloy of
adding copper to aluminum-silicon alloy.
|
In general, it can be used at the
fusion point of aluminum alloyed tin (AC type).
|
|
TA-107
|
BA4047
|
Its fusion point is especially low
at the work progress temperature of aluminum-silicon
alloy.
|
Because its fusion point is low, it
is used to weld the thin board of aluminum and aluminum
alloys. It can be also used for a narrow gap part.
|
|
TA-110
|
-
|
After the anode oxidation treatment,
the color of its basic material around the welded
part is not altered. Its flowability is fine.
|
|